YOU HERE: Alloy Standards -> Copper - all grades OR Alloy Standards -> / EN 13601 / EN 13600 / EN 13602 / EN 1652 / EN 1976 / EN 13599 / EN 13605 / EN 12165 / EN 12420 / EN 13148 |
Cu-ETP ( CW004A )
Grade : | Cu-ETP |
Number: | CW004A |
Classification: | Unalloyed copper |
Density | 8.9 g/cm ³ |
Standard: | EN 13601: 2002 Copper and copper alloys. Copper rod, bar and wire for general electrical purposesEN 13600: 2002 Copper and copper alloys. Seamless copper tubes for electrical purposesEN 13602: 2002 Copper and copper alloys. Drawn, round copper wire for the manufacture of electrical conductorsEN 1652: 1998 Copper and copper alloys. Plate, sheet, strip and circles for general purposesEN 1976: 1998 Copper and copper alloys. Cast unwrought copper productsEN 13599: 2002 Copper and copper alloys. Copper plate, sheet and strip for electrical purposesEN 13605: 2002 Copper and copper alloys. Copper profiles and profiled wire for electrical purposesEN 12165: 1998 Copper and copper alloys. Wrought and unwrought forging stockEN 12420: 1999 Copper and copper alloys. ForgingsEN 13148: 2001 Copper and copper alloys. Hot-dip tinned strip |
Equivalent grades: | Go here |
Chemical composition % of grade Cu-ETP ( CW004A )
Cu including Ag < 0.015%; O < 0.06% is permitted |
Cu | Pb | O | Bi | Others |
min 99.9 | max 0.005 | max 0.04 | max 0.0005 | total 0.03 |
Mechanical properties of grade Cu-ETP ( CW004A )
|
Rm - Tensile strength (MPa) (R200) | 200 |
|
Rm - Tensile strength (MPa) (R240) | 240-300 |
|
Rm - Tensile strength (MPa) (R290) | 290-360 |
|
Rp0.2 0.2% proof strength (MPa) (R200) | 120 |
|
Rp0.2 0.2% proof strength (MPa) (R240) | 180 |
|
Rp0.2 0.2% proof strength (MPa) (R290) | 250 |
|
A - Min. elongation at fracture (%) (R200) | 35 |
|
A - Min. elongation at fracture (%) (R240) | 15 |
|
A - Min. elongation at fracture (%) (R290) | 6 |
|
A - Min. elongation Lo = 100mm (%) (R200) | 25 |
|
A - Min. elongation Lo = 50mm (%) (R240) | 8 |
|
A - Min. elongation Lo = 50mm (%) (R290) | 4 |
Vickers hardness ( HV): (H065) | 65 - 95 |
Vickers hardness ( HV): (H090) | 90 - 110 |
Vickers hardness ( HV): (H035) (R200) | 35 - 65 |
Properties Cu-ETP
Volume resistivity = 0.01724 - 0.01786 Ω*mm²/m ; |
Equivalent grades of grade Cu-ETP ( CW004A )Warning! Only for reference
EU EN | USA- | GermanyDIN,WNr | JapanJIS | FranceAFNOR | EnglandBS | ItalyUNI | SwedenSS | PolandPN | CzechiaCSN | AustriaONORM | RussiaGOST | InterISO |
Cu-ETP | | | | | | | | | | | | |
Casting process
GS | Sand casting |
GM | Permanent mould casting |
GZ | Centrifugal casting |
GC | Continuous casting |
GP | Pressure die casting |
Material conditions
R | Material condition designated by the minimum value of tensile strength requirement for the product with mandatory tensile strength and elongation requirements |
H | Material condition designated by the minimum value of hardness requirement for the product with mandatory hardness requirements |
Mechanical properties
ReH | Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d elasticite minimale |
Rm | Tensile strength / Zugfestigkeit / Resistance a la traction |
A | Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal |
J | Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc |